Polymer Property : Specific Gravity = 1.026 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.026 g/cc
1.026 g/cc
Northstar Polymers PBA-031 Polyether Curing Agent
Information provided by Northstar Polymers.
Specific Gravity 1.026 g/cc

@Temperature 23.9 °C
1.026 g/cc

@Temperature 75.0 °F
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding  (discontinued **)
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Specific Gravity 1.026 g/cc
1.026 g/cc
Dow VORANOL™ CP 4702 Polyol
VORANOL™ CP 4702 polyol is a high reactivity, capped triol, polyether polyol especially designed for the production of molded flexible foam. It is normally used in all TDI or TDI/MDI blend formula..