Dow SPECTRIM™ MM 310-A Isocyanate

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name SPECTRIM™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow SPECTRIM™ MM 310-A Isocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SPECTRIM™ MM 310-A specialty isocyanate is a component of SPECTRIM™ MM 310 reaction moldable polymer.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
Viscosity 180 cP

@Temperature 25.0 °C
180 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point >= 204 °C
>= 399 °F