Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Nordel® NDR 3722P EPDM Hydrocarbon Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® NDR 3722P EPDM Hydrocarbon Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NDR 3722P is a semicrystalline, very low diene containing polymer with low viscosity for good processability. The low unsaturation provides excellent long term thermal and UV stability. It is specially designed for medium voltage wire and cable applications. It can also be used in peroxide cured molded and other extruded applications. NDR 3722P is developmental and made via INSITE™ technology.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.880 g/cc
0.0318 lb/in³
ASTM D297
Volatiles <= 0.40 %
<= 0.40 %
Total Volatiles; DuPont Dow PQ-E-007
Mooney Viscosity 20

@Temperature 125 °C
20

@Temperature 257 °F
ML 1 + 4; ASTM D1646
Ash <= 0.10 %
<= 0.10 %
ASTM D5667
Descriptive Properties Value Comments
ENB 0.5 mass%
ASTM D6047
Ethylene 70.5 mass%
ASTM D3900
Molecular Weight Distribution Medium
DuPont Dow PQ-E-034 and 036
Product Form Pellets
Propylene 29 mass%
ASTM D3900
Residual Transition Metal Max 10 ppm
DuPont Dow
Copyright © lookpolymers.com All Rights Reserved