Material Notes:
Description: NDR 37060.02 is a medium viscosity, medium ethylene EPDM grade having a moderate cure rate that is suited to applications where low modulus, good elongation, as well as heat and weather aging resistance are required. NDR 37060.02 is produced in a unique granular form that contains some carbon black.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D297
Volatiles <= 0.40 %
<= 0.40 %
Total Volatiles; DuPont Dow EPRG-21
Mooney Viscosity 78

@Temperature 125 °C
78

@Temperature 257 °F
ML 1 + 4; ASTM D1646
Descriptive Properties Value Comments
Carbon Black Content (N650) 30 phr
DuPont Dow EPRG-2
ENB 2.2 mass%
ASTM D6047
Ethylene 68 mass%
ASTM D3900
Users viewing this material also viewed the following: