Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow H110-02N Polypropylene Homopolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow H110-02N Polypropylene Homopolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewContains a nucleating agentHigh clarityGood melt strengthComplies with U.S. FDA 21 CFR 177.1520 (c)3.2a, Canadian HPFB No ObjectionDOW H110-02N Polypropylene Resin is intended for use in extrusion and thermoforming processes. It is especially suited in applications where improved melt strength and clarity are desired.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa
5110 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus, 1% Secant 1590 MPa
231000 psi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Temperature 0.000 °C
0.599 ft-lb/in

@Temperature 32.0 °F
ASTM D256A
0.507 J/cm

@Temperature 23.0 °C
0.950 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 161 °C
322 °F
DSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Haze 14 %
14 %
ASTM D1003
Copyright © lookpolymers.com All Rights Reserved