Dow Corning XIAMETER® PMCPPMX-200 300,000CS Silicone Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPPMX-200 300,000CS Silicone Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 200 FLUID 300,000CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, color cosmetic, and antiperspirant / deodorant applications. INCI Name: DimethiconeInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Viscosity Measure 300000 cSt
300000 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point >= 230 °C
>= 446 °F
Open Cup
Optical Properties Metric English Comments
Refractive Index 1.4035
1.4035