Dow Corning XIAMETER® PMCPOFX-8600 Fluid

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPOFX-8600 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 8600 HYDROPHILIC SOFTENER. An organofunctional silicone fluid designed to provide durable softness without compromising any hydrophilic nature of the fabric.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 3000 - 12000 cP
3000 - 12000 cP
Dynamic
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Amino Content (%) 0.65-0.7
Color Opaque