Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® 9416/30E KIT PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 9416/30E KIT PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30 Durometer, two-part, 1 to 1 mix, opaque, injection mold grade silicone rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 7.0002 MPa
1015.3 psi
Elongation at Break 800 %
800 %
Tear Strength 20.02 kN/m
114.2 pli
Compression Set 18 %
18 %
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Copyright © lookpolymers.com All Rights Reserved