Dow Corning 3629

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3629.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two Part LSR SystemInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.144 g/cc

@Temperature 25.0 °C
1.144 g/cc

@Temperature 77.0 °F
Viscosity 8000 cP
8000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 27
27
Tensile Strength, Ultimate 1.300 MPa
188.5 psi
Elongation at Break 275 %
275 %
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color white
Mix Ratio (X:1) 10
Base to Catalyst ETN