Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning 347 EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 347 EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® 347 Emulsion is a concentrated emulsion of hydroxyl end-blocked dimethyl silicone fluid. A stable, water-dilutable nonionic polydimethylsiloxane, Dow Corning 347 Emulsion is highly surface active to provide good release, lubricity, water repellency and gloss in numerous industrial and specialty chemical applications. Diluted with water and applied by spraying or dipping, Dow Corning 347 Emulsion leaves a thin but highly effective silicone release film on mold surfaces. In most cases, this heatstable film does not carbonize at temperatures which quickly destroy organic mold release agents, does not build up on molds, and does not discolor rubber or plastic parts. Dow Corning 347 Emulsion has demonstrated exceptional stability. A small amount of rust inhibitor is formulated into Dow Corning 347 Emulsion to resist rusting in the concentrated form. Because of the reactive chemical sites on the polydimethylsiloxane, Dow Corning 347 Emulsion can be reacted with various substrates. Crosslinking agents and catalysts can be used to obtain a more resinous coating.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
pH 6.0 - 8.5
6.0 - 8.5
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Active Content (%) 60
Appearance liquid
Color milky white
Non-Ionic yes
Solvent water
Users viewing this material also viewed the following: