Corning 7059 Barium Borosilicate Glass

Category Ceramic , Glass , Optical , Oxide , Silicon Oxide
Manufacturer Corning Incorporated
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Corning 7059 Barium Borosilicate Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features a low alkali content of less than 0.3%. In thin sheet form, it is an ideal substrate glass that is also used for low-end LCD applications. Also available crushed/powdered for sealing and other uses.Information provided by Corning Incorporated.
Physical Properties Metric English Comments
Density 2.76 g/cc
0.0997 lb/in³
Thermal Properties Metric English Comments
CTE, linear 4.60 µm/m-°C

@Temperature 0.000 - 300 °C
2.56 µin/in-°F

@Temperature 32.0 - 572 °F
Softening Point 844 °C
1550 °F
Annealing Point 639 °C
1180 °F
Strain Point 593 °C
1100 °F
Optical Properties Metric English Comments
Refractive Index 1.5333

@Wavelength 589.3 nm
1.5333

@Wavelength 589.3 nm