Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 844 °C | 1550 °F | |
Corning 7059 Barium Borosilicate Glass Features a low alkali content of less than 0.3%. In thin sheet form, it is an ideal substrate glass that is also used for low-end LCD applications. Also available crushed/powdered for sealing and o.. |
|||
Softening Point | 846 °C | 1550 °F | |
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |