Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ConocoPhillips Hydroclear® Fluid

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear PowerTran Fluid, formulated from premium hydrocracked base stock, is a multipurpose fluid for farm equipment, off-highway machinery, and industrial tractors whose transmissions, final drives, wet brakes and clutches, and hydraulics are supplied from a common fluid reservoir. Hydroclear PowerTran Fluid offers outstanding low-temperature performance. It reduces wear, rust, and corrosion. Special additives protect seals to prevent leakage. Friction modifiers ensure that wet brakes and transmission clutch packs function properly. Hydroclear PowerTran Fluid offers excellent load-carrying capacity and oxidation control in extended-service applications. Hydroclear PowerTran Fluid is recommended for Caterpillar TO-2, Denison HF-2 and HF-1, Eaton, Sperry-Vickers and Sundstrand Hydraulic fluid applications. It meets or exceeds specifications set forth by John Deere, Case IH and New Holland.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 30.2 °
30.2 °
Viscosity 37400 cP

@Temperature -35.0 °C
37400 cP

@Temperature -31.0 °F
Viscosity Measurement 143
143
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 61.4 cSt
61.4 cSt
Kinematic Viscosity at 100°C (212°F) 9.8 cSt
9.8 cSt
ASTM Color 1.5
1.5
Thermal Properties Metric English Comments
Pour Point -38.9 °C
-38.0 °F
Flash Point 225 °C
437 °F
Users viewing this material also viewed the following: