Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 37400 cP @Temperature -35.0 °C |
37400 cP @Temperature -31.0 °F |
|
ConocoPhillips Hydroclear® Fluid Description: Conoco Hydroclear PowerTran Fluid, formulated from premium hydrocracked base stock, is a multipurpose fluid for farm equipment, off-highway machinery, and industrial tractors whose tran.. |