Chosun Refractories ASM-31 Air-Setting Mortar

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories ASM-31 Air-Setting Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Grain Size 75 µm
75 µm
40% <= 0.075 mm
300 µm
300 µm
10% >= 0.30 mm
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.981 MPa

@Temperature 110 °C,
Time 86400 sec
142 psi

@Temperature 230 °F,
Time 24.0 hour
2.4525 MPa

@Temperature 1000 °C,
Time 10800 sec
355.71 psi

@Temperature 1830 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 30 %
30 %
Fe2O3 >= 3.0 %
>= 3.0 %
Descriptive Properties Value Comments
Main Applications SK31 Bricks
Refractoriness (SK) 31=