Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories AMCM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories AMCM-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 1000 °C, Time 10800 sec |
142 psi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories APM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASCM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASCM-S Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-32 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-34 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories BM-2W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 1400 °C, Time 10800 sec |
142 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories BM-3 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories BM-3W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | <= 0.981 MPa @Temperature 110 °C, Time 86400 sec |
<= 142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HM-A Special Mortar for Sliding Gate Valve Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-31 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 110 °C, Time 86400 sec |
142 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories BM-1W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 0.981 MPa @Temperature 500 °C, Time 10800 sec |
142 psi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories BM-1W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |