Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.87 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.104 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.88 g/cc

@Temperature 1000 °C,
Time 10800 sec
0.104 lb/in³

@Temperature 1830 °F,
Time 3.00 hour
2.94 g/cc

@Temperature 110 °C,
Time 86400 sec
0.106 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Porosity 21 %

@Temperature 110 °C,
Time 86400 sec
21 %

@Temperature 230 °F,
Time 24.0 hour
23 %

@Temperature 1500 °C,
Time 10800 sec
23 %

@Temperature 2730 °F,
Time 3.00 hour
23.5 %

@Temperature 1000 °C,
Time 10800 sec
23.5 %

@Temperature 1830 °F,
Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0034335 GPa

@Temperature 110 °C,
Time 86400 sec
0.49799 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0044145 GPa

@Temperature 1000 °C,
Time 10800 sec
0.64028 ksi

@Temperature 1830 °F,
Time 3.00 hour
0.01226 GPa

@Temperature 1500 °C,
Time 10800 sec
1.779 ksi

@Temperature 2730 °F,
Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.200 %

@Temperature 1500 °C,
Time 10800 sec
-0.200 %

@Temperature 2730 °F,
Time 3.00 hour
-0.0600 %

@Temperature 1000 °C,
Time 10800 sec
-0.0600 %

@Temperature 1830 °F,
Time 3.00 hour
-0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 95 %
95 %
MgO 3.0 %
3.0 %
SiO2 1.0 %
1.0 %
Descriptive Properties Value Comments
Main Applications Blast Furnace Iron runner for desiliconized
Material Required for Estimating (kg/?) 2,800