Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D792
Melt Flow 0.75 g/10 min
0.75 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ASTM D648