Chosun Refractories 1260BLANKET Blanket

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories 1260BLANKET Blanket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Shrinkage 1.3 %

@Temperature 1000 °C,
Time 86400 sec
1.3 %

@Temperature 1830 °F,
Time 24.0 hour
1.8 %

@Temperature 1100 °C,
Time 86400 sec
1.8 %

@Temperature 2010 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 47.1 %
47.1 %
SiO2 52.3 %
52.3 %
Descriptive Properties Value Comments
Typical applications Furnace Linings, Heat seals, Packing, Fire Protection, Noise reduction, Filter Material