Information provided by China Tungsten
Physical Properties Metric English Comments
Density 6.60 - 7.20 g/cc
0.238 - 0.260 lb/in³
Component Elements Properties Metric English Comments
Carbon, C 0.50 - 2.0 %
0.50 - 2.0 %
total
Copper, Cu 60 - 69 %
60 - 69 %
Iron, Fe 0.50 %
0.50 %
Lead, Pb 2.0 - 4.0 %
2.0 - 4.0 %
Other <= 1.5 %
<= 1.5 %
Tin, Sn 5.0 - 7.0 %
5.0 - 7.0 %
Zinc, Zn 5.0 - 7.0 %
5.0 - 7.0 %
Descriptive Properties Value Comments
Oil %, Min 18
Skin Hardness (HR) 20-50