Polymer Property : Density = 0.238 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 6.60 g/cc
0.238 lb/in³
PSM Industries Ferro-TiC® PK Maraging Steel
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Comb..
Density 6.60 g/cc
0.238 lb/in³
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized
Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is ..
Density 6.60 g/cc
0.238 lb/in³
Indium Corp. Indalloy 176 Zinc Solder Alloy
Information Provided by Indium Corporation
Density 6.60 - 7.20 g/cc
0.238 - 0.260 lb/in³
China Tungsten ST2170 PM Antifriction Parts
Information provided by China Tungsten
Density 6.60 g/cc
0.238 lb/in³
Sintered
Ametek P316L P/M Stainless Steel, Sintered from 6.30 g/cc Green Density
P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu..
Density 6.60 g/cc
0.238 lb/in³
Ametek P304L P/M Stainless Steel, Sintered from 6.5 g/cc Green Density
Powder apparent bulk density 2.7 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for ..
Density 6.60 g/cc
0.238 lb/in³
PSM Industries Ferro-TiC® C Medium Alloy Tool Steel
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce..
Density 6.60 g/cc
0.238 lb/in³
Ametek P303L P/M Stainless Steel, Sintered from 6.5 g/cc Green Density
Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for ..