Material Notes:
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.22 g/cc
0.297 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 331 MPa
48000 psi
Tensile Strength, Yield 110 MPa
16000 psi
Elongation at Break 15 %
15 %
Component Elements Properties Metric English Comments
Aluminum, Al 0.50 %
0.50 %
Copper, Cu 55 - 60 %
55 - 60 %
Iron, Fe 0.35 %
0.35 %
Lead, Pb 1.5 - 2.5 %
1.5 - 2.5 %
Other, total 0.50 %
0.50 %
Tin, Sn 0.30 %
0.30 %
Zinc, Zn 35.85 - 41.85 %
35.85 - 41.85 %
as balance