Material Notes:
FeaturesChevron THF W is a high quality, multifunctional fluid, specially formulated for low temperature use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other equipment employing a common fluid reservoir.It is formulated with high quality base stocks, a viscosity index improver, oxidation and corrosion inhibitors, antiwear and film strength additives, an antifoaming agent, and a pour point depressant.ApplicationsChevron THF W is specifically formulated to meet the requirements of Jophn Deere J20D.It is recommended for use in equipment that operates at low ambient temperatures and as a multifunctional fluid in all types of farm tractors and equipment. It can also be used in any application which calls for the following OEM lubricant specifications:AGCO-improved power fluid 821XLJohn Deere-J20DNew Holland-ESN-M2C134-A/B/C/D, FNHA 2 C 201Massey Ferguson-M1135, M1141, M1143White Farm Equipment-Q-1826Case Corporation-JIC-143, JIC-145, MS 1206, MS 1207, MS 1209, MS 1210 (TCH)Oliver-Type 55Minneapolis-Moline-FluidsCaterpillar-TO-2Renk-Bus Automatic Transmission Fluid 873, 874 A/BKubota-UDTInternational Harvester-B6Deutz-Allis 821XL
Physical Properties Metric English Comments
API Gravity 31.9 °
31.9 °
Brookfield Viscosity 17000 cP

@Temperature -40.0 °C
17000 cP

@Temperature -40.0 °F
Viscosity Measurement 185
185
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 174.2 SUS
174.2 SUS
Saybolt Viscosity at 210°F 50.6 SUS
50.6 SUS
Kinematic Viscosity at 40°C (104°F) 34.4 cSt
34.4 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.3 cSt
7.3 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -48.0 °C
-54.4 °F
ASTM D97
Flash Point 214 °C
417 °F
ASTM D92
Descriptive Properties Value Comments
Color Pale