ChevronTexaco RPM® Arctic Gear Lubricant

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco RPM® Arctic Gear Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron RPM Arctic Gear Lubricant is a multipurpose, heavy duty automotive gear lubricant designed to meet the severe demands of cold weather operations. It is formulated with ISOSYN® base stocks and compounded with extreme pressure, antiwear, corrosion inhibition, rust preventive, and foam suppressant additives, as well as a shear stable viscosity index improver. This additive package is a new generation sulfur-phosphorus system with improved thermal stability, gear spalling protection, and antiwear performance.Chevron RPM Arctic Gear Lubricant is designed to provide maximum wear protection for automotive gear sets operating in extremely cold conditions, where fluidity of the lubricant is critical to protect gears and bearings. Low viscosity hastens the release of entrained air in the lubricant at low temperatures, thereby providing a better oil film on moving parts.ApplicationsChevron RPM Arctic Gear Lubricant is recommended for all automotive rear axle and manual transmission gears operating in severe arctic climates, or where the manufacturer recommends a viscosity range lighter than conventional SAE 80W 90 or SAE 85W 140 gear lubricants.Chevron RPM Arctic Gear Lubricant meets the requirements of API Service Categories GL4, GL-5 and MT-1.It is engineered to pass the performance requirements of SAE J 2360 (formerly known as MIL PRF-2105E).
Physical Properties Metric English Comments
API Gravity 28.6 °
28.6 °
Brookfield Viscosity 120000 cP

@Temperature -40.0 °C
120000 cP

@Temperature -40.0 °F
Saybolt Viscosity at 100°F 475 SUS
475 SUS
Saybolt Viscosity at 210°F 87 SUS
87 SUS
Kinematic Viscosity at 40°C (104°F) 94 cSt
94 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 16.8 cSt
16.8 cSt
ASTM D445
Mechanical Properties Metric English Comments
Timken Test 22700 g
50.0 lb
Thermal Properties Metric English Comments
Pour Point -45.0 °C
-49.0 °F
ASTM D97
Descriptive Properties Value Comments
Channel Point °C -50
Corrosion, Copper Strip Test 3h 1B at 120°C