Material Notes:
Texaco Geotex Ashless is a high quality, bright stock-free, ashless, dispersant-type gas engine oil. It is manufactured using selected paraffinic base oils and an additive package containing a dispersant, wear inhibitor and oxidation inhibitor.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221879; MSDS Number: 8677
Physical Properties Metric English Comments
API Gravity 30.2 °
30.2 °
Viscosity Measurement 127
127
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 104 cSt
104 cSt
Kinematic Viscosity at 100°C (212°F) 13.4 cSt
13.4 cSt
Thermal Properties Metric English Comments
Pour Point -27.0 °C
-16.6 °F
Flash Point 250 °C
482 °F
Component Elements Properties Metric English Comments
Phosphorous, P 0.087 %
0.087 %
Zinc, Zn <= 0.0010 %
<= 0.0010 %
Chemical Properties Metric English Comments
Acid Value 0.30
0.30
ASTM D 664
Total Base Number 1.5
1.5
ASTM D2896