Cadi Cu-Tungsten (55%) Copper Alloy

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Cadi Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cadi Cu-Tungsten (55%) Copper Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specified for electrode and electrode inserts for many flash and butt welding applications. This grade is specified when higher electrical and thermal conductivity are required.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 12.6 g/cc
0.455 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B >= 72

@Diameter <=25.4 mm
>= 72

@Diameter <=1.00 in
Component Elements Properties Metric English Comments
Copper, Cu 45 %
45 %
Tungsten, W 55 %
55 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.00000383 ohm-cm
<= 0.00000383 ohm-cm
Calculated from Min 45 %IACS
Descriptive Properties Value Comments
RMWA Class 10