Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000383 ohm-cm | 0.00000383 ohm-cm | (45% IACS) |
CMW® ELKONITE® 10W3 Copper Tungsten RWMA Class 11 Electrical contacts resistant to arcing, power transformer switches, resistance / projection welding electrodes, and EDM electrodesInformation provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000383 ohm-cm | 0.00000383 ohm-cm | (45% IACS) |
CMW® ELKONITE® 3150 Silver Tungsten Carbide contact material ASTM B663 Table 2, Class B For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000383 ohm-cm | 0.00000383 ohm-cm | (45% IACS) |
CMW® ELKONITE® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000383 ohm-cm | 0.00000383 ohm-cm | (45% IACS) |
CMW® ELKONITE® TC5 Tungsten Carbide Copper material For wiping and arcing electrical contacts and light duty welding tips.Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000383 ohm-cm | 0.00000383 ohm-cm | (45% IACS) |
CMW® THERMKON® 83 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Electrical Resistivity | <= 0.00000383 ohm-cm | <= 0.00000383 ohm-cm | Calculated from Min 45 %IACS, up to 3" diameter/any thickness |
Cadi 1 MOLD-MOR™ A very hard heat treatable copper alloy with moderate electrical conductivity. C18000 offers excellent value for the properties it offers. C18000 is a viable substitute for C17500 and C17510 for m.. |
|||
Electrical Resistivity | <= 0.00000383 ohm-cm | <= 0.00000383 ohm-cm | Calculated from Min 45 %IACS, up to 3" diameter/any thickness |
Cadi 10 MOLD-MOR™ A Copper Nickel Silicon Chromium Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company. |
|||
Electrical Resistivity | <= 0.00000383 ohm-cm | <= 0.00000383 ohm-cm | Calculated from Min 45 %IACS, up to 3" diameter/any thickness |
Cadi 2 MOLD-MOR™ A very hard heat treatable beryllium-copper alloy with moderate electrical conductivity. C17510 can be utilized when a combination of very good mechanical strength along with moderate electrical an.. |
|||
Electrical Resistivity | <= 0.00000383 ohm-cm | <= 0.00000383 ohm-cm | Calculated from Min 45 %IACS, up to 3" diameter/any thickness |
Cadi 20 MOLD-MOR™ A Beryllium Copper Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company. |
|||
Electrical Resistivity | <= 0.00000383 ohm-cm | <= 0.00000383 ohm-cm | Calculated from Min 45 %IACS, up to 3" diameter/any thickness |
Cadi C17500 Copper Alloy Information provided by Cadi Company. |
|||
Electrical Resistivity | <= 0.00000383 ohm-cm | <= 0.00000383 ohm-cm | Calculated from Min 45 %IACS |
Cadi Cu-Tungsten (55%) Copper Alloy Specified for electrode and electrode inserts for many flash and butt welding applications. This grade is specified when higher electrical and thermal conductivity are required.Information provided.. |