Material Notes:
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 15.56 g/cc
0.5621 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90 - 100
90 - 100
Component Elements Properties Metric English Comments
Silver, Ag 22 %
22 %
Tungsten, W 78 %
78 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000325 - 0.00000358 ohm-cm
0.00000325 - 0.00000358 ohm-cm
Calculated from 48-53 %IACS