Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000325 - 0.00000358 ohm-cm | 0.00000325 - 0.00000358 ohm-cm | Calculated from 48-53 %IACS |
Cadi 20WS Tungsten Silver Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |
|||
Electrical Resistivity | 0.00000325 - 0.00000358 ohm-cm | 0.00000325 - 0.00000358 ohm-cm | Calculated from 48-53 %IACS |
Cadi 3WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |