CMW® D154F Pre-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer CMW Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® D154F Pre-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For electrical contacts; resistant to welding and high surge currents.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.08 g/cc
0.3642 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 71 - 90
71 - 90
71 (annealed) - 90 (worked)
Tensile Strength, Ultimate 276 MPa
40000 psi
Annealed
324 MPa
47000 psi
Worked
Thermal Properties Metric English Comments
Melting Point <= 980 °C
<= 1800 °F
Liquidus 980 °C
1800 °F
Component Elements Properties Metric English Comments
CdO 13.3 %
13.3 %
Silver, Ag 86.7 %
86.7 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000230 ohm-cm
0.00000230 ohm-cm
(75% IACS)