Breplast Bretene LD BT Thermoplastic Composite, 50% LD + 50% PP

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP)
Manufacturer Breplast S.P.A.
Trade Name Bretene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Breplast Bretene LD BT Thermoplastic Composite, 50% LD + 50% PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Melt Flow 0.80 - 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 - 1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Color Dark Grey