Braskem PH 0130 HOMO Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PH 0130 HOMO Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PH 0130 is a low melt flow rate homopolymer with a general purpose additive package. This resin is designed for blow molding and extrusion. PH 0130 features excellent processability and stiffness/impact strength balance. Its applications include: bottles for mineral water, drinks, and cosmetics; general use; ropes; flat and corrugated sheets; profiles; tear tape; and tapes in general.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM-D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM-D638
Elongation at Yield 10 %
10 %
ASTM-D638
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM-D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
ASTM-D648
Vicat Softening Point 156 °C

@Load 1.02 kg
313 °F

@Load 2.25 lb
ASTM-D1525