Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 156 °C | 313 °F | B |
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525B |
SABIC PP 504P Polypropylene Homopolymer for Raffia Applications Product Description: PP 504P is specially developed for producing stretched tapes with the following features:Consistent processabilityEasy orientationLow water carry overGood mechanical properties.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EX9332T PC (Europe-Africa-Middle East) LEXAN* EX9332T polycarbonate resin, MVR (300C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retadant, mold release, UV stabilized, transparent, translucent and opaque colors. Materi.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525 |
PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermofor.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ASTM D1525-97 |
Ipiranga Petrochem PH 0321 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 156 °C @Load 1.02 kg |
313 °F @Load 2.25 lb |
GOST 15088 |
Sibur H250 GP Polypropylene Homopolymer Polypropylene homopolymer with narrow molecular weight distribution. It features high fluidity, an optimal stabilization package and balanced physical and mechanical properties.general purpose produ.. |
|||
Vicat Softening Point | 156 °C | 313 °F | |
Styron CALIBRE™ 200 10 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Vicat Softening Point | 156 °C | 313 °F | |
Styron CALIBRE™ 300 10 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 156 °C | 313 °F | A (10N); ISO 306 |
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ISO 306 |
Unipetrol PP MONSTEN® MA 230 Polypropylene Homopolymer Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 156 °C | 313 °F | ISO 306 |
Unipetrol PP MONSTEN® NB 112 Polypropylene Homopolymer Applications include injection molding and fibers. Basic and anti-gasfading stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 156 °C | 313 °F | B50 (50°C/h 50N); ISO 306 |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Vicat Softening Point | 156 °C | 313 °F | 10 N; ASTM D1525 |
Braskem CP 401 HC Injection Molding Polypropylene Description: CP 401HC is a medium melt flow rate heterophasic copolymer, specially designed to achieve high stiffness/impact strength balance. This product offers good surface appearance and process.. |
|||
Vicat Softening Point | 156 °C @Load 1.02 kg |
313 °F @Load 2.25 lb |
ISO 306 |
Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Vicat Softening Point | 156 °C | 313 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 GB6 POM 30% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Vicat Softening Point | 156 °C | 313 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 M POM Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info.. |
|||
Vicat Softening Point | 156 °C | 313 °F | 10 N; ASTM D1525 |
Braskem H 103 Extrusion Coating Polypropylene Homopolymer Description: H 103 is a high melt flow rate additivated homopolymer used for general purposes. The product exhibits excellent processing performance on injection moulding applications. Applications:.. |
|||
Vicat Softening Point | 156 °C | 313 °F | ISO 306 |
Unipetrol PP MONSTEN® GB 107 Polypropylene Homopolymer Made for injection molding. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 156 °C | 313 °F | ISO 306 |
Unipetrol PP MONSTEN® FC 110 Polypropylene Homopolymer Applications include injection molding, packaging films, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 156 °C @Load 1.02 kg |
313 °F @Load 2.25 lb |
A50; ISO 306 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |