Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBABLEND M 13/26 PA12 functional compound, polymer bonded magnet

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Barlog Plastics
Trade Name KEBABLEND
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBABLEND M 13/26 PA12 functional compound, polymer bonded magnet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA 12 mod.Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527-1
Elongation at Break 1.9 %
1.9 %
ISO 527-1
Tensile Modulus 10.0 GPa
1450 ksi
ISO 527-1
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Resin Type PA 12 mod.