Bapolene® 4082NA Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 4082NA Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene 4082NA is a homopolymer polypropylene designed for fast-cycle molding applications. It is nucleated and contains antistat. Material meets the requirements of US FDA 21 CFR1777.1520.Applications: Rigid packaging and housewares.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D-1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D-638
Elongation at Yield 7.0 %
7.0 %
ASTM D-638
Flexural Modulus, 1% Secant 1551 MPa
225000 psi
ASTM D-790A
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution