Material Notes:
No. 20 is an air-setting mortar, gray in color, for use where extra hard air-set strength is desired. It is not recommended for laying insulating fire brick. Used up to 2700°F for setting hard brick with a rubbed joint and for washcoating hard brick. When desired to use old fire brick as a patching material or monolithic fill, No. 20 is thinned with water and the crushed brick added. Note: Coating IFB is rarely advisable.Information provided by BNZ Materials Inc.
Physical Properties Metric English Comments
Bulk Density 1.86 g/cc
0.0671 lb/in³
Dipping, 10% H2O
1.94 g/cc
0.0700 lb/in³
As received
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0324 GPa
4.70 ksi
Mortar
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1480 °C
2700 °F
Shrinkage 5.1 %
5.1 %
Permanent Linear Change at Use Limit
Component Elements Properties Metric English Comments
Al2O3 5.1 %
5.1 %
Na2O 3.3 %
3.3 %
SiO2 90.8 %
90.8 %