Polymer Property : Bulk Density = 1.86 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.86 g/cc
0.0671 lb/in³
Dipping, 10% H2O
BNZ Materials Zelie No. 20 Mortar
No. 20 is an air-setting mortar, gray in color, for use where extra hard air-set strength is desired. It is not recommended for laying insulating fire brick. Used up to 2700°F for setting hard bric..
Bulk Density 1.86 g/cc
0.0671 lb/in³
Powder
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia
Castable ceramic with high dielectric and physical strength.