Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BNZ Materials 2645LI Insulating Aggregate

Category Ceramic , Oxide , Silicon Oxide
Manufacturer BNZ Materials, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BNZ Materials 2645LI Insulating Aggregate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for installation by various methods including gunning, casting or slap-troweling. Each product is specifically formulated to economically obtain the desired properties for the application and service temperature for which it is intended.Information provided by BNZ Materials Inc.
Physical Properties Metric English Comments
Density 0.721 g/cc
0.0260 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 1.90 MPa
275 psi
Thermal Properties Metric English Comments
Shrinkage 0.80 %

@Temperature 1427 °C,
Time 86400 sec
0.80 %

@Temperature 2601 °F,
Time 24.0 hour
Permanent Linear Change; ASTM C210
4.4 %

@Temperature 1482 °C,
Time 86400 sec
4.4 %

@Temperature 2700 °F,
Time 24.0 hour
Permanent Linear Change; ASTM C210
Component Elements Properties Metric English Comments
Al2O3 37.6 %
37.6 %
CaO 0.00 %
0.00 %
Fe2O3 0.60 %
0.60 %
MgO 0.00 %
0.00 %
Na2O 0.20 %
0.20 %
Includes K<sub>2</sub>O
SiO2 59.4 %
59.4 %
TiO2 1.2 %
1.2 %
Users viewing this material also viewed the following: