Formula: C5H8O2CAS: 140-88-5Description: Acrylic acid ester suitable for the production of polymers and as a feedstock for syntheses.Applications: Ethyl acrylate forms homopolymers and copolymers. Copolymers of ethyl acrylate can be prepared with acrylic acid and its salts, amides and esters, methacrylates, acrylonitrile, maleates, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene, unsaturated polyesters and drying oils. Ethyl acrylate is also an important feedstock for chemical syntheses because it readily undergoes addition reactions with many organic and inorganic compounds.Information provided by BASF
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
Viscosity 0.55 cP
0.55 cP
Molecular Weight 100.1 g/mol
100.1 g/mol
Vapor Pressure 0.00390 bar
2.93 torr
Thermal Properties Metric English Comments
Specific Heat Capacity 1.98 J/g-°C
0.473 BTU/lb-°F
of Liquid
Melting Point -72.0 °C
-97.6 °F
Freezing Point
Boiling Point 100 °C
212 °F
Optical Properties Metric English Comments
Refractive Index 1.404
1.404
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
ASTM D203
Descriptive Properties Value Comments
Assay >99.7%
Color <10
APHA, ASTM D1209
Heat of Polymerization 655 kJ/kg
Latent Heat of Evaporation at Boiling Point 346.1 kJ/kg