Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.00390 bar | 2.93 torr | |
BASF Ethyl Acrylate Formula: C5H8O2CAS: 140-88-5Description: Acrylic acid ester suitable for the production of polymers and as a feedstock for syntheses.Applications: Ethyl acrylate forms homopolymers and copolymers. .. |