Material Notes:
Formula: C4H7NOCAS: 616-45-5Description: 2-Pyrrolidone Distilled is a colorless to yellow liquid, with a faint amine-like odor. It is miscible in water.Synonyms: 2P, Pyrrolidone, 2-Pyrrolidinone, 2-Oxopyrrolidine, 2-Tetrahydropyrrolone, 4-Aminobutyric acid lactam, ButyrolactamApplications: Intermediate used in Formulation aids, Industrial chemicals, Initial product for chemical syntheses, Inks and PharmaceuticalInformation provided by BASF
Physical Properties Metric English Comments
Density 1.103 g/cc
0.03985 lb/in³
Molecular Weight 85.1 g/mol
85.1 g/mol
Thermal Properties Metric English Comments
Melting Point 25.0 °C
77.0 °F
Freezing Point
25.5 °C
77.9 °F
Boiling Point 250 °C
482 °F
Flash Point 138 °C
280 °F
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99.5%
Color <50
APHA, DIN EN 1557
Composition 1,4-Butanediol
<0.1%
Gamma Butyrolactone
<0.1%
Ignition Temperature 390°C