Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 25.5 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 25.5 °C
77.9 °F
BASF 2-Pyrrolidone Distilled
Formula: C4H7NOCAS: 616-45-5Description: 2-Pyrrolidone Distilled is a colorless to yellow liquid, with a faint amine-like odor. It is miscible in water.Synonyms: 2P, Pyrrolidone, 2-Pyrrolidinone, 2-..