Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Austin Novel Materials Texalan® 785A PCL TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 785A PCL TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Physical Properties Metric English Comments
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
ISO 7619
Tensile Strength >= 32.0 MPa
>= 4640 psi
ISO 37
Tensile Stress >= 5.00 MPa

@Strain 100 %
>= 725 psi

@Strain 100 %
ISO 37
>= 9.00 MPa

@Strain 300 %
>= 1310 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 550 %
>= 550 %
ISO 37
Tear Strength >= 70.0 kN/m
>= 399 pli
ISO 34
K Factor (Wear Factor) <= 60
<= 60
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 25 %

@Temperature 70.0 °C
<= 25 %

@Temperature 158 °F
ISO 815