Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 9.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 9.00 MPa

@Strain 0.349 %,
Time 360000 sec
1310 psi

@Strain 0.349 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Tensile Stress 9.00 MPa

@Strain 50.0 %
1310 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 9.00 MPa

@Strain 27.59 %,
Temperature 90.0 °C
1310 psi

@Strain 27.59 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress >= 9.00 MPa

@Strain 300 %
>= 1310 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 282A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 590A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 795A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 395A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 398A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 300 %
>= 1310 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 385A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 300 %
>= 1310 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 785A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Copyright © lookpolymers.com All Rights Reserved