Ashley Polymers Ashlene® C1176 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® C1176 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These are also available with UV, designated by -3. For release, add R. These are all flame retardant grades developed for various applications such as electrical, electronic, lighting, computer, appliance, business equipment and communications.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Moisture Absorption at Equilibrium 0.34 %
0.34 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 15 - 17 g/10 min
15 - 17 g/10 min
Cond. O
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Ultimate 61.0 MPa
8850 psi
ATSM D638
Elongation at Break 75 %
75 %
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Users viewing this material also viewed the following: