Physical Properties Metric English Comments
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antist..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® MFA® P6010 Perfluoropolymer
Hyflon® MFA P6010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® MFA® P6310 Perfluoropolymer
Hyflon® MFA P6310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA P7310 Perfluoroalkoxy (PFA)
Hyflon® PFA P7310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti..
Melt Flow 12 - 17 g/10 min

@Load 5.00 kg,
Temperature 365 °C
12 - 17 g/10 min

@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU)
Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA)
Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti..
Melt Flow 11 - 17 g/10 min

@Load 2.16 kg,
Temperature 280 °C
11 - 17 g/10 min

@Load 4.76 lb,
Temperature 536 °F
Zeon Chemicals Zeonor® 1060R Cyclo-Olefin Polymer
Zeonor 1020R shall be in the form of pellets.
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
Daikin NEOFLON AP-221SH PFA Semiconductor Grade
NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries.
Melt Flow 15 - 17 g/10 min
15 - 17 g/10 min
Cond. 300/1.2
Ashley Polymers Ashlene® 1021 Polycarbonate
A general purpose injection molding grade, natural resin. Also available as: 1021R (with release), 1023 (with UV stabilizers); 1023R (with release and UV stabilizers).Data provided by the manufactu..
Melt Flow 15 - 17 g/10 min
15 - 17 g/10 min
Ashley Polymers Ashlene® 1105 Polycarbonate, 5-7% Glass Reinforced
A general purpose foamable injection molding grade resin with 5-7% glass reinforcement.Data provided by the manufacturer
Melt Flow 15 - 17 g/10 min

@Load 1.20 kg,
Temperature 300 °C
15 - 17 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Cond. O
Ashley Polymers Ashlene® 1621 Polycarbonate
A general purpose injection molding grade, natural resin, UL approved. Also available as: 1621R (with release); 1623 (with UV stabilizers); 1623R (with release and UV stabilizers).Data provided by ..
Melt Flow 15 - 17 g/10 min
15 - 17 g/10 min
Cond. O
Ashley Polymers Ashlene® C1176 Polycarbonate
These are also available with UV, designated by -3. For release, add R. These are all flame retardant grades developed for various applications such as electrical, electronic, lighting, computer, ..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Melt Flow 15 - 17 g/10 min
15 - 17 g/10 min
Cond. 300/1.2
Ashley Polymers Ashlene® P1021R Polycarbonate
A prime general purpose injection molding grade, natural resin with easy mold release.Data provided by the manufacturer