Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Leona® 90G55 55% Glass Filled Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 60% Glass Fiber Filled
Manufacturer Asahi Kasei
Trade Name Leona®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Leona® 90G55 55% Glass Filled Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Enhanced strength and stiffness; with 55% GF. Excellent appearance and weatherability. Color- BlackApplications:Exterior automotive parts Information provided by Asahi Kasei
Copyright © lookpolymers.com All Rights Reserved