Asahi Glass Lumiflon LF-916N Solvent Soluble Fluoropolymer

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer Asahi Glass Company
Trade Name Lumiflon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Lumiflon LF-916N Solvent Soluble Fluoropolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability between the Fluoroethylene and Alkyl Vinyl Ether gives excellent weathering and a high chemical resistance. LF-916N is designed for weather resistant coatings, and has been used in the Aerospace and automotive fields.Information provided by Asahi Glass Company, Inc.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved