Material Notes:
Design/Construction:Side 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.531 g/cc
0.05531 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 1570 microns
62.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Silicone Property; ASTM D2240
Tensile Strength 4.83 MPa
700 psi
Silicone Property; ASTM D412
Elongation at Break 200 %
200 %
Silicone Property; ASTM D412
Compression Set 5.0 %

@Temperature 149 °C,
Time 79200 sec
5.0 %

@Temperature 300 °F,
Time 22.0 hour
Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Off White
Total Product Weight (oz/yd2) 71
Arlon SQA-TMS-025