Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 4.83 MPa | >= 700 psi | |
Garlock Bay State 22 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, smooth rotocured finish. It conforms easily to uneven flange surfaces.Information pr.. |
|||
Tensile Strength | 4.83 MPa | 700 psi | |
Teknor Apex Elexar® EL 3954-62 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | 4.83 MPa | 700 psi | Silicone Property; Arlon SQA-TMS-008 |
Arlon 32980XA015 0.015" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon 51591R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data .. |
|||
Tensile Strength | 4.83 MPa | 700 psi | Silicone Property; ASTM D412 |
Arlon 51866R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Tensile Strength | 4.83 MPa | 700 psi | Silicone Property; ASTM D412 |
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 920-05Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: ½” RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not requi.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 920-07Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon 920-07Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 920-20Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon 920-20Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 930-125Rxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon 940-07Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wr.. |
|||
Tensile Strength | 4.83 MPa | 700 psi | Silicone Property; Arlon SQA-TMS-008 |
Arlon 99322B015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Static dissipating siliconeDesign/Construction:Interleave: 0.0025" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Chemlock 607This data repres.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave Design/Construction:Cross Section Type: TriangularArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for subsequent.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon LW201Xxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon LW202Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon LW202Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon LW202Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon LW301Rxx-P1 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon LW6015Xxx-P0 0.060" (1.52 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Tensile Strength | 4.83 MPa | 700 psi | Silicone Property; ASTM D412 |
Arlon R37152W062 0.062" (1.57 mm) Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInform.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon 912-10RXX-P0 0.012" (0.305 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 920-15Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 930-10Xxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 940-07Bxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Compound Property |
Arlon 940-07Bxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Tensile Strength | >= 4.83 MPa | >= 700 psi | Product Property |
Arlon 940-10Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Tensile Strength | 4.83 MPa | 700 psi | ASTM D412 |
Arlon R35232B020 0.020" (0.508 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |
|||
Tensile Strength | 4.83 MPa | 700 psi | ASTM D412 |
Arlon R35232B085 0.085" (2.16 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |